Screen the first available source row for each property. Results may use typical or estimated values and are not design allowables. Inspect the displayed conditions and full record; unreported values cannot satisfy a filter.
105 Screening CandidatesFiltered by parametric engineering constraints
| Designation • Canonical Grade | Subfamily | Conductivity | Thermal Cond. | Yield Strength & Context | Tensile (UTS) | Status | Actions |
|---|---|---|---|---|---|---|---|
| C11000 ETP CopperElectrolytic Tough Pitch | Pure Copper | 101 % IACSTYPICAL · 20 °C · CDA Physical Properties section: Measured at 68°F (20°C), volume and weight basis | 391.15 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties section: Measured at 68°F (20°C). Raw: Btu/sq ft/ft hr/°F | 206.8 MPaTYPICAL · 1/4 Hard (H01) · Flat Products · 0.025 in · 20 °C · Section Size: 0.025 in; Yield strength at 0.5% extension under load | 289.6 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 in · 20 °C · Section Size: 0.04 in | VERIFIED | |
| C10100 Oxygen-Free Electronic (OFE) CopperOxygen-Free Electronic | Pure Copper | 101 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 101.0 % IACS at 68°F (20°C) | 391.15 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 226.0 Btu/(ft·hr·°F) (391.15 W/(m·K) at 20°C) | 248.2 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 289.6 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C10200 Oxygen-Free (OF) CopperOxygen-Free | Pure Copper | 101 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 101.0 % IACS at 68°F (20°C) | 391.15 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 226.0 Btu/(ft·hr·°F) (391.15 W/(m·K) at 20°C) | 248.2 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 289.6 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C10300 Oxygen-Free Extra Low Phosphorus (OFXLP) CopperOxygen-Free Extra Low Phosphorus | Deoxidized Copper | 99 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 99.0 % IACS at 68°F (20°C) | 385.95 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 223.0 Btu/(ft·hr·°F) (385.95 W/(m·K) at 20°C) | 248.2 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 289.6 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C12000 DLP CopperPhosphorus-Deoxidized Low Residual Phosphorus | Deoxidized Copper | 98 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 98.0 % IACS at 68°F (20°C) | 385.95 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 223.0 Btu/(ft·hr·°F) (385.95 W/(m·K) at 20°C) | 248.2 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 289.6 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C12200 DHP CopperPhosphorus-Deoxidized High Residual Phosphorus | Deoxidized Copper | 85 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 85.0 % IACS at 68°F (20°C) | 339.22 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 196.0 Btu/(ft·hr·°F) (339.22 W/(m·K) at 20°C) | 206.8 MPaTYPICAL · 1/4 Hard (H01) · Flat Products · 0.25 · 20 °C · Section Size: 0.25; Section Size: 0.25 in; Yield strength at 0.5% extension under load | 289.6 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C14500 Tellurium CopperTellurium Copper | Free-Machining Copper | 93 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 93.0 % IACS at 68°F (20°C) | 354.8 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 205.0 Btu/(ft·hr·°F) (354.8 W/(m·K) at 20°C) | 275.8 MPaTYPICAL · 1/2 Hard (H02) · Rod · 1 · 20 °C · Section Size: 1; Cold Work: 20%; Section Size: 1 in; Yield strength at 0.5% extension under load | 262 MPaTYPICAL · 1/2 Hard (H02) · Rod · 0.25 · 20 °C · Section Size: 0.25; Cold Work: 20%; Section Size: 0.25 in | VERIFIED | |
| C14700 Sulfur CopperSulfur Copper | Free-Machining Copper | 95 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 95.0 % IACS at 68°F (20°C) | 373.84 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 216.0 Btu/(ft·hr·°F) (373.84 W/(m·K) at 20°C) | 268.9 MPaTYPICAL · 1/2 Hard (H02) · Rod · 2 · 20 °C · Section Size: 2; Section Size: 2 in; Yield strength at 0.5% extension under load | 289.6 MPaTYPICAL · 1/2 Hard (H02) · Rod · 2 · 20 °C · Section Size: 2; Section Size: 2 in | VERIFIED | |
| C17200 Beryllium Copper (Alloy 25)Alloy 25 | Beryllium Copper | 22 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 22.0 % IACS at 68°F (20°C) | 107.31 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 62.0 Btu/(ft·hr·°F) (107.31 W/(m·K) at 20°C) | 1206.6 MPaTYPICAL · 1/2 Hard and Precipitation Heat Treated (TH02) · Flat Products · 0.188 · 20 °C · Section Size: 0.188; Section Size: 0.188 in; Yield strength at 0.5% extension under load | 1344.5 MPaTYPICAL · 1/2 Hard and Precipitation Heat Treated (TH02) · Flat Products · 0.188 · 20 °C · Section Size: 0.188; Section Size: 0.188 in | VERIFIED | |
| C17500 Beryllium Copper (Alloy 10)Alloy 10 | Beryllium Copper | 45 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 45.0 % IACS at 68°F (20°C) | 207.69 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 120.0 Btu/(ft·hr·°F) (207.69 W/(m·K) at 20°C) | 655 MPaTYPICAL · Hard and Precipitation Heat Treated (TH04) · Flat Products · 20 °C · Yield strength at 0.5% extension under load | 758.4 MPaTYPICAL · Hard and Precipitation Heat Treated (TH04) · Flat Products · 20 °C | VERIFIED | |
| C17510 Beryllium Copper (Alloy 3)Alloy 3 | Beryllium Copper | 48 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 48.0 % IACS at 68°F (20°C) | 207.69 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 120.0 Btu/(ft·hr·°F) (207.69 W/(m·K) at 20°C) | 744.6 MPaTYPICAL · 1/2 Hard and Precipitation Heat Treated (TH02) · Flat Products · 20 °C · Yield strength at 0.5% extension under load | 792.9 MPaTYPICAL · 1/2 Hard and Precipitation Heat Treated (TH02) · Flat Products · 20 °C | VERIFIED | |
| C19400 High-Strength Modified Copper (HSM Copper)HSM Copper | High-Performance Copper Alloys | 65 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 65.0 % IACS at 68°F (20°C) | 259.61 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 150.0 Btu/(ft·hr·°F) (259.61 W/(m·K) at 20°C) | 365.4 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 413.7 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C26000 Cartridge Brass 70/30Cartridge Brass 70/30 | Cartridge Brass | 28 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 28.0 % IACS at 68°F (20°C) | 121.15 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 70.0 Btu/(ft·hr·°F) (121.15 W/(m·K) at 20°C) | 275.8 MPaTYPICAL · 1/4 Hard (H01) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 427.5 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C26800 Yellow Brass 66%Yellow Brass 66% | Yellow Brass | 27 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 27.0 % IACS at 68°F (20°C) | 115.96 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 67.0 Btu/(ft·hr·°F) (115.96 W/(m·K) at 20°C) | 344.7 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 420.6 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C27000 Yellow Brass 65%Yellow Brass 65% | Yellow Brass | 27 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 27.0 % IACS at 68°F (20°C) | 115.96 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 67.0 Btu/(ft·hr·°F) (115.96 W/(m·K) at 20°C) | 344.7 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 420.6 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C27200 Yellow Brass 63%Yellow Brass 63% | Yellow Brass | 27.6 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 27.6 % IACS at 68°F (20°C) | 115.96 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 67.0 Btu/(ft·hr·°F) (115.96 W/(m·K) at 20°C) | 379.2 MPaTYPICAL · Hard Drawn (H80) · Tube · 0.065 · 20 °C · Section Size: 0.065; Section Size: 0.065 in; Yield strength at 0.5% extension under load | 510.2 MPaTYPICAL · Hard Drawn (H80) · Tube · 0.065 · 20 °C · Section Size: 0.065; Section Size: 0.065 in | VERIFIED | |
| C28000 Muntz Metal 60/40Muntz Metal | Yellow Brass | 28 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 28.0 % IACS at 68°F (20°C) | 122.88 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 71.0 Btu/(ft·hr·°F) (122.88 W/(m·K) at 20°C) | 344.7 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 482.6 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C36000 Free-Cutting BrassFree-Cutting Brass | Free-Machining Brass | 26 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 26.0 % IACS at 68°F (20°C) | 115.96 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 67.0 Btu/(ft·hr·°F) (115.96 W/(m·K) at 20°C) | 117.2 MPaTYPICAL · 1/2 Hard (H02) · Bar · 1.5 · 20 °C · Section Size: 1.5; Section Size: 1.5 in; Yield strength at 0.5% extension under load | 310.3 MPaTYPICAL · 1/2 Hard (H02) · Bar · 1.5 · 20 °C · Section Size: 1.5; Section Size: 1.5 in | VERIFIED | |
| C46400 Naval BrassNaval Brass | Naval Brass | 26 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 26.0 % IACS at 68°F (20°C) | 115.96 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 67.0 Btu/(ft·hr·°F) (115.96 W/(m·K) at 20°C) | 172.4 MPaTYPICAL · As Hot Rolled (M20) · Flat Products · 1 · 20 °C · Section Size: 1; Section Size: 1 in; Yield strength at 0.5% extension under load | 482.6 MPaTYPICAL · 1/4 Hard (H01) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C51000 Phosphor Bronze 5% APhosphor Bronze 5% Grade A | Phosphor Bronze | 15 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 15.0 % IACS at 68°F (20°C) | 69.23 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 40.0 Btu/(ft·hr·°F) (69.23 W/(m·K) at 20°C) | 372.3 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 20 °C · Yield strength at 0.5% extension under load | 455.1 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 20 °C | VERIFIED | |
| C52100 Phosphor Bronze 8% CPhosphor Bronze 8% Grade C | Phosphor Bronze | 13 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 13.0 % IACS at 68°F (20°C) | 62.31 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 36.0 Btu/(ft·hr·°F) (62.31 W/(m·K) at 20°C) | 441.3 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 530.9 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C54400 Free-Machining Phosphor Bronze (B-2)Phosphor Bronze B-2 | Phosphor Bronze | 19 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 19.0 % IACS at 68°F (20°C) | 86.54 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 50.0 Btu/(ft·hr·°F) (86.54 W/(m·K) at 20°C) | 275.8 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 399.9 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C61400 Aluminum Bronze DAluminum Bronze D | Aluminum Bronze | 14 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 14.0 % IACS at 68°F (20°C) | 67.5 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 39.0 Btu/(ft·hr·°F) (67.5 W/(m·K) at 20°C) | 413.7 MPaTYPICAL · Hard (H04) · Flat Products · 0.125 · 20 °C · Section Size: 0.125; Section Size: 0.125 in; Yield strength at 0.5% extension under load | 613.6 MPaTYPICAL · Hard (H04) · Flat Products · 0.125 · 20 °C · Section Size: 0.125; Section Size: 0.125 in | VERIFIED | |
| C63000 Nickel-Aluminum Bronze (AMS 4640)Nickel-Aluminum Bronze | Aluminum Bronze | 7 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 7.0 % IACS at 68°F (20°C) | 39.11 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 22.6 Btu/(ft·hr·°F) (39.11 W/(m·K) at 20°C) | 344.7 MPaTYPICAL · As Hot Extruded (M30) · Bar · 3 · 20 °C · Section Size: 3; Section Size: 3 in; Yield strength at 0.5% extension under load | 620.5 MPaTYPICAL · As Hot Extruded (M30) · Bar · 3 · 20 °C · Section Size: 3; Section Size: 3 in | VERIFIED | |
| C63200 Nickel-Aluminum Bronze (Naval Alloy)Naval Nickel-Aluminum Bronze | Aluminum Bronze | 7 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 7.0 % IACS at 68°F (20°C) | 34.61 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 20.0 Btu/(ft·hr·°F) (34.61 W/(m·K) at 20°C) | 310.3 MPaTYPICAL · Light Anneal (O50) · Forgings · 5 · 20 °C · Section Size: 5; Section Size: 5 in; Yield strength at 0.5% extension under load | 689.5 MPaTYPICAL · Light Anneal (O50) · Forgings · 5 · 20 °C · Section Size: 5; Section Size: 5 in | VERIFIED | |
| C65500 High-Silicon Bronze AHigh-Silicon Bronze A | Silicon Bronze | 7 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 7.0 % IACS at 68°F (20°C) | 36.35 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 21.0 Btu/(ft·hr·°F) (36.35 W/(m·K) at 20°C) | 241.3 MPaTYPICAL · 1/4 Hard (H01) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load | 537.8 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in | VERIFIED | |
| C70600 Copper-Nickel 90/10Copper-Nickel 90/10 | Copper-Nickel (Cupronickel) | 9 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 9.0 % IACS at 68°F (20°C) | 45 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 26.0 Btu/(ft·hr·°F) (45.0 W/(m·K) at 20°C) | 172.4 MPaTYPICAL · Hard (H04) · Bar · 20 °C · Yield strength at 0.5% extension under load | 344.7 MPaTYPICAL · Hard (H04) · Bar · 20 °C | VERIFIED | |
| C71500 Copper-Nickel 70/30Copper-Nickel 70/30 | Copper-Nickel (Cupronickel) | 4.6 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 4.6 % IACS at 68°F (20°C) | 29.42 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 17.0 Btu/(ft·hr·°F) (29.42 W/(m·K) at 20°C) | — | 379.2 MPaTYPICAL · As Hot Rolled (M20) · Flat Products · 1 · 20 °C · Section Size: 1; Section Size: 1 in | VERIFIED | |
| C93200 Bearing Bronze (SAE 660)SAE 660 | Bearing Bronze | 12 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 12.0 % IACS at 68°F (20°C) | 58.15 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 33.6 Btu/(ft·hr·°F) (58.15 W/(m·K) at 20°C) | 96.5 MPaTYPICAL · As Centrifugal Cast (M02) · As Centrifugal Cast · 20 °C · Yield strength at 0.5% extension under load | 206.8 MPaTYPICAL · As Centrifugal Cast (M02) · As Centrifugal Cast · 20 °C | VERIFIED | |
| C95400 Aluminum Bronze 9CAluminum Bronze 9C | Aluminum Bronze | 13 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 13.0 % IACS at 68°F (20°C) | 58.67 W/(m·K)TYPICAL · 20 °C · CDA Physical Properties: Thermal conductivity 33.9 Btu/(ft·hr·°F) (58.67 W/(m·K) at 20°C) | 206.8 MPaTYPICAL · As Centrifugal Cast (M02) · As Centrifugal Cast · 20 °C · Yield strength at 0.5% extension under load | 517.1 MPaTYPICAL · As Centrifugal Cast (M02) · As Centrifugal Cast · 20 °C | VERIFIED | |
| 17-4 PH (630) Stainless Steel | Precipitation Hardening | — | 17.9 W/(m·K)TYPICAL · H900 · 149 °C | 1275.5 MPaTYPICAL · H900 · Bar · LONGITUDINAL · Typical longitudinal bar properties; section dimensions and test temperature not stated in this table. Not minimum requirements. | 1379 MPaTYPICAL · H900 · Bar · LONGITUDINAL · Typical longitudinal bar properties; section dimensions and test temperature not stated in this table. Not minimum requirements. | VERIFIED | |
| 409 Stainless Steel | Ferritic | — | 25.8 W/(m·K)TYPICAL · 100 °C | ≥ 170 MPaMINIMUM · Annealed · Sheet and Strip | ≥ 380 MPaMINIMUM · Annealed · Sheet and Strip | VERIFIED | |
| SAE 1008 Carbon Steel | Carbon Steel | — | 51.9 W/(m·K)TYPICAL · 100 °C | ≥ 168.9 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 303.4 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1010 Carbon Steel | Carbon Steel | — | 51.9 W/(m·K)TYPICAL · 100 °C | ≥ 179.3 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 324.1 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1018 Carbon Steel | Carbon Steel | — | 51.9 W/(m·K)TYPICAL · 100 °C | ≥ 220.6 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 399.9 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1020 Carbon Steel | Carbon Steel | — | 51.9 W/(m·K)TYPICAL · 100 °C | ≥ 206.8 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 379.2 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1025 Carbon Steel | Carbon Steel | — | 51.5 W/(m·K)TYPICAL · 100 °C | ≥ 220.6 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 399.9 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1030 Carbon Steel | Carbon Steel | — | 51 W/(m·K)TYPICAL · 100 °C | ≥ 258.6 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 468.8 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1035 Carbon Steel | Carbon Steel | — | 50.7 W/(m·K)TYPICAL · 100 °C | ≥ 272.3 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 496.4 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1040 Carbon Steel | Carbon Steel | — | 50 W/(m·K)TYPICAL · 100 °C | ≥ 289.6 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 524 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1045 Carbon Steel | Carbon Steel | — | 49.8 W/(m·K)TYPICAL · 100 °C | ≥ 310.3 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 565.4 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1050 Carbon Steel | Carbon Steel | — | 49 W/(m·K)TYPICAL · 100 °C | ≥ 341.3 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 620.5 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1060 Carbon Steel | Carbon Steel | — | 48.5 W/(m·K)TYPICAL · 100 °C | ≥ 372.3 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 675.7 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1070 Carbon Steel | Carbon Steel | — | 48 W/(m·K)TYPICAL · 100 °C | ≥ 386.1 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 703.3 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1080 Carbon Steel | Carbon Steel | — | 48 W/(m·K)TYPICAL · 100 °C | ≥ 424 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | ≥ 772.2 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated. | VERIFIED | |
| SAE 1095 Carbon Steel | Carbon Steel | — | 48 W/(m·K)TYPICAL · 100 °C | ≥ 380 MPaMINIMUM · Spheroidize Annealed Bar · Bar | ≥ 655 MPaMINIMUM · Spheroidize Annealed Bar · Bar | VERIFIED | |
| SAE 4130 Alloy Steel | Alloy Steel | — | 42.7 W/(m·K)TYPICAL · 100 °C | ≥ 435 MPaMINIMUM · Normalized Bar · Bar | ≥ 670 MPaMINIMUM · Normalized Bar · Bar | VERIFIED | |
| SAE 4140 Alloy Steel | Alloy Steel | — | 42.6 W/(m·K)TYPICAL · 100 °C | ≥ 740 MPaMINIMUM · Quenched and tempered (voestalpine supply) · Bar · 10–100 mm · voestalpine supply properties for the stated section range; source does not specify test temperature. Not extrapolated to other products or heat treatments. | 930–1080 MPaRANGE · Quenched and tempered (voestalpine supply) · Bar · 10–100 mm · voestalpine supply properties for the stated section range; source does not specify test temperature. Not extrapolated to other products or heat treatments. | VERIFIED | |
| SAE 4142 Alloy Steel | Alloy Steel | — | 42.6 W/(m·K)TYPICAL · 100 °C | ≥ 640 MPaMINIMUM · Normalized Bar · Bar | ≥ 980 MPaMINIMUM · Normalized Bar · Bar | VERIFIED | |
| SAE 4150 Alloy Steel | Alloy Steel | — | 42.6 W/(m·K)TYPICAL · 100 °C | ≥ 430 MPaMINIMUM · Annealed Bar · Bar | ≥ 730 MPaMINIMUM · Annealed Bar · Bar | VERIFIED | |
| SAE 4340 Alloy Steel | Alloy Steel | — | 44.5 W/(m·K)TYPICAL · 100 °C | ≥ 470 MPaMINIMUM · Annealed Bar · Bar | ≥ 745 MPaMINIMUM · Annealed Bar · Bar | VERIFIED | |
| SAE 4620 Alloy Steel | Alloy Steel | — | 46.6 W/(m·K)TYPICAL · 100 °C | ≥ 360 MPaMINIMUM · Normalized Bar - Core Properties · Bar | ≥ 600 MPaMINIMUM · Normalized Bar - Core Properties · Bar · Core properties for carburizing grade. | VERIFIED | |
| SAE 5120 Alloy Steel | Alloy Steel | — | 46.6 W/(m·K)TYPICAL · 100 °C | ≥ 340 MPaMINIMUM · Normalized Bar - Core Properties · Bar | ≥ 580 MPaMINIMUM · Normalized Bar - Core Properties · Bar · Core properties for carburizing grade. | VERIFIED | |
| SAE 5140 Alloy Steel | Alloy Steel | — | 46 W/(m·K)TYPICAL · 100 °C | ≥ 410 MPaMINIMUM · Annealed Bar · Bar | ≥ 640 MPaMINIMUM · Annealed Bar · Bar | VERIFIED | |
| SAE 5160 Alloy Steel | Alloy Steel | — | 46 W/(m·K)TYPICAL · 100 °C | ≥ 400 MPaMINIMUM · Annealed Bar · Bar | ≥ 720 MPaMINIMUM · Annealed Bar · Bar | VERIFIED | |
| SAE 6150 Alloy Steel | Alloy Steel | — | 46 W/(m·K)TYPICAL · 100 °C | ≥ 410 MPaMINIMUM · Annealed Bar · Bar | ≥ 670 MPaMINIMUM · Annealed Bar · Bar | VERIFIED | |
| SAE 8620 Alloy Steel | Alloy Steel | — | 46.6 W/(m·K)TYPICAL · 100 °C | ≥ 380 MPaMINIMUM · Normalized Bar (870°C) - Core Properties · Bar · Core mechanical properties. | ≥ 630 MPaMINIMUM · Normalized Bar (870°C) - Core Properties · Bar · Core mechanical properties. Case hardening properties require a specified carburizing and quenching cycle. | VERIFIED | |
| SAE 8630 Alloy Steel | Alloy Steel | — | 46.6 W/(m·K)TYPICAL · 100 °C | ≥ 450 MPaMINIMUM · Normalized Bar · Bar | ≥ 720 MPaMINIMUM · Normalized Bar · Bar | VERIFIED | |
| SAE 8640 Alloy Steel | Alloy Steel | — | 46.6 W/(m·K)TYPICAL · 100 °C | ≥ 415 MPaMINIMUM · Annealed Bar · Bar | ≥ 690 MPaMINIMUM · Annealed Bar · Bar | VERIFIED | |
| SAE 8740 Alloy Steel | Alloy Steel | — | 46.6 W/(m·K)TYPICAL · 100 °C | ≥ 415 MPaMINIMUM · Annealed Bar · Bar | ≥ 690 MPaMINIMUM · Annealed Bar · Bar | VERIFIED | |
| SAE 9310 Alloy Steel | Alloy Steel | — | 46 W/(m·K)TYPICAL · 100 °C | ≥ 585 MPaMINIMUM · Normalized Bar - Core Properties · Bar | ≥ 825 MPaMINIMUM · Normalized Bar - Core Properties · Bar · Core properties for heavy-duty carburizing grade. | VERIFIED | |
| SAE 52100 Alloy Steel | Alloy Steel | — | 46.6 W/(m·K)TYPICAL · 100 °C | ≥ 380 MPaMINIMUM · Spheroidize Annealed Bar · Bar | ≥ 620 MPaMINIMUM · Spheroidize Annealed Bar · Bar | VERIFIED | |
| 201 Stainless Steel | Austenitic | — | 16.2 W/(m·K)TYPICAL · 100 °C | ≥ 310 MPaMINIMUM · Annealed · Sheet and Strip | ≥ 655 MPaMINIMUM · Annealed · Sheet and Strip | VERIFIED | |
| 202 Stainless Steel | Austenitic | — | — | ≥ 310 MPaMINIMUM · Annealed · Sheet and Strip | ≥ 620 MPaMINIMUM · Annealed · Sheet and Strip | VERIFIED | |
| 301 Stainless Steel | Austenitic | — | 16.3 W/(m·K)TYPICAL · 100 °C | ≥ 276 MPaMINIMUM · Annealed · Sheet and Strip | ≥ 758 MPaMINIMUM · Annealed · Sheet and Strip | VERIFIED | |
| 302 Stainless Steel | Austenitic | — | 16.2 W/(m·K)TYPICAL · 100 °C | ≥ 205 MPaMINIMUM · Annealed · Sheet and Strip | ≥ 515 MPaMINIMUM · Annealed · Sheet and Strip | VERIFIED | |
| 303 Stainless Steel | Austenitic | — | 16.2 W/(m·K)TYPICAL · 100 °C | ≥ 205 MPaMINIMUM · Cold Finished Annealed Bar · Bar | ≥ 515 MPaMINIMUM · Cold Finished Annealed Bar · Bar | VERIFIED | |
| 304 Stainless Steel | Austenitic | — | 16.3 W/(m·K)TYPICAL · 100 °C | ≥ 206.8 MPaMINIMUM · ASTM requirements (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. | ≥ 517.1 MPaMINIMUM · ASTM requirements (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. | VERIFIED | |
| 304L Stainless Steel | Austenitic | — | 16.3 W/(m·K)TYPICAL · 100 °C | ≥ 172.4 MPaMINIMUM · ASTM requirements (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. | ≥ 482.6 MPaMINIMUM · ASTM requirements (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. | VERIFIED | |
| 305 Stainless Steel | Austenitic | — | 16.2 W/(m·K)TYPICAL · 100 °C | ≥ 170 MPaMINIMUM · Annealed · Sheet and Strip | ≥ 485 MPaMINIMUM · Annealed · Sheet and Strip | VERIFIED | |
| 309 Stainless Steel | Austenitic | — | 15.6 W/(m·K)TYPICAL · 100 °C | ≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip | ≥ 515 MPaMINIMUM · Annealed · Plate, Sheet and Strip | VERIFIED | |
| 310 Stainless Steel | Austenitic | — | 14.2 W/(m·K)TYPICAL · 100 °C | ≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip | ≥ 515 MPaMINIMUM · Annealed · Plate, Sheet and Strip | VERIFIED | |
| 316 Stainless Steel | Austenitic | — | 14.6 W/(m·K)TYPICAL · 100 °C | ≥ 206.8 MPaMINIMUM · ASTM requirements at room temperature (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. Source specifies room temperature without a numeric temperature. | ≥ 517.1 MPaMINIMUM · ASTM requirements at room temperature (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. Source specifies room temperature without a numeric temperature. | VERIFIED | |
| 316L Stainless Steel | Austenitic | — | 14.6 W/(m·K)TYPICAL · 100 °C | ≥ 172.4 MPaMINIMUM · ASTM requirements at room temperature (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. Source specifies room temperature without a numeric temperature. | ≥ 482.6 MPaMINIMUM · ASTM requirements at room temperature (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. Source specifies room temperature without a numeric temperature. | VERIFIED | |
| 321 Stainless Steel | Austenitic | — | 16.1 W/(m·K)TYPICAL · 100 °C | ≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip | ≥ 515 MPaMINIMUM · Annealed · Plate, Sheet and Strip | VERIFIED | |
| 347 Stainless Steel | Austenitic | — | 16.1 W/(m·K)TYPICAL · 100 °C | ≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip | ≥ 515 MPaMINIMUM · Annealed · Plate, Sheet and Strip | VERIFIED | |
| 410 Stainless Steel | Martensitic | — | 24.9 W/(m·K)TYPICAL · 100 °C | ≥ 205 MPaMINIMUM · Annealed · Bar and Sheet | ≥ 450 MPaMINIMUM · Annealed · Bar and Sheet | VERIFIED | |
| 420 Stainless Steel | Martensitic | — | 24.9 W/(m·K)TYPICAL · 100 °C | ≥ 345 MPaMINIMUM · Annealed · Bar and Strip | ≥ 585 MPaMINIMUM · Annealed · Bar and Strip | VERIFIED | |
| 1050 Aluminum1050A | Wrought Aluminum Alloys | — | 222 W/(m·K)TYPICAL | ≥ 20 MPaMINIMUM · O Temper · Sheet · 0.2mm to 6.0mm | 65–95 MPaRANGE · O Temper · Sheet · 0.2mm to 6.0mm | VERIFIED | |
| 3103 AluminumEN AW-3103 | Wrought Aluminum Alloys | — | 160 W/(m·K)TYPICAL | ≥ 115 MPaMINIMUM · H14 Temper · Sheet · 0.2mm to 6.0mm | 140–180 MPaRANGE · H14 Temper · Sheet · 0.2mm to 6.0mm | VERIFIED | |
| 5005 AluminumEN AW-5005 | Wrought Aluminum Alloys | — | 201 W/(m·K)TYPICAL | ≥ 110 MPaMINIMUM · H34 Temper · Sheet · 0.2mm to 12.5mm | 145–185 MPaRANGE · H34 Temper · Sheet · 0.2mm to 12.5mm | VERIFIED | |
| 5083 AluminumEN AW-5083 | Wrought Aluminum Alloys | — | 121 W/(m·K)TYPICAL | ≥ 125 MPaMINIMUM · O / H111 Temper · Sheet · 0.2mm to 6.3mm | 275–350 MPaRANGE · O / H111 Temper · Sheet · 0.2mm to 6.3mm | VERIFIED | |
| 5251 AluminumEN AW-5251 | Wrought Aluminum Alloys | — | 149 W/(m·K)TYPICAL | ≥ 60 MPaMINIMUM · O Temper · Sheet & Plate · 0.2mm to 50.0mm | 160–200 MPaRANGE · O Temper · Sheet & Plate · 0.2mm to 50.0mm | VERIFIED | |
| 5454 AluminumEN AW-5454 | Wrought Aluminum Alloys | — | 134 W/(m·K)TYPICAL | ≥ 85 MPaMINIMUM · O / H111 Temper · Sheet · 0.2mm to 6.0mm | 215–265 MPaRANGE · O / H111 Temper · Sheet · 0.2mm to 6.0mm | VERIFIED | |
| 5754 AluminumEN AW-5754 | Wrought Aluminum Alloys | — | 147 W/(m·K)TYPICAL | ≥ 80 MPaMINIMUM · H111 Temper · Sheet · 0.2mm to 6.0mm | 190–240 MPaRANGE · H111 Temper · Sheet · 0.2mm to 6.0mm | VERIFIED | |
| 6005A AluminumEN AW-6005A | Wrought Aluminum Alloys | — | 188 W/(m·K)TYPICAL | ≥ 225 MPaMINIMUM · T6 Temper · Extrusions · up to 5mm | ≥ 270 MPaMINIMUM · T6 Temper · Extrusions · up to 5mm | VERIFIED | |
| 6026 AluminumEN AW-6026 | Wrought Aluminum Alloys | — | 138 W/(m·K)TYPICAL | ≥ 360 MPaMINIMUM · T9 Temper · Extruded and Drawn Bar | ≥ 390 MPaMINIMUM · T9 Temper · Extruded and Drawn Bar | VERIFIED | |
| 6060 AluminumEN AW-6060 | Wrought Aluminum Alloys | — | 200 W/(m·K)TYPICAL | ≥ 120 MPaMINIMUM · T5 Temper · Extrusions · Up to 150mm Dia., 15mm WT tube, 5mm WT profiles | ≥ 160 MPaMINIMUM · T5 Temper · Extrusions · Up to 150mm Dia., 15mm WT tube, 5mm WT profiles | VERIFIED | |
| 6082 AluminumEN AW-6082 | Wrought Aluminum Alloys | — | 180 W/(m·K)TYPICAL | ≤ 85 MPaMAXIMUM · O Temper · Sheet · 0.4mm to 6.0mm | ≤ 150 MPaMAXIMUM · O Temper · Sheet · 0.4mm to 6.0mm | VERIFIED | |
| 6101 AluminumEN AW-6101 | Wrought Aluminum Alloys | — | 218 W/(m·K)TYPICAL | ≥ 170 MPaMINIMUM · T6 Temper · Extruded Bar · up to 150mm | ≥ 200 MPaMINIMUM · T6 Temper · Extruded Bar · up to 150mm | VERIFIED | |
| 6106 AluminumEN AW-6106 | Wrought Aluminum Alloys | — | 190 W/(m·K)TYPICAL | ≥ 200 MPaMINIMUM · T6 Temper · Extruded Profiles · up to 10mm WT | ≥ 250 MPaMINIMUM · T6 Temper · Extruded Profiles · up to 10mm WT | VERIFIED | |
| 6262 AluminumEN AW-6262 | Wrought Aluminum Alloys | — | 172 W/(m·K)TYPICAL | ≥ 240 MPaMINIMUM · T6 Temper · Extrusions · up to 200mm Dia | ≥ 260 MPaMINIMUM · T6 Temper · Extrusions · up to 200mm Dia | VERIFIED | |
| 1100 AluminumAA 1100 | Wrought Aluminum Alloys | 59 % IACSTYPICAL · O Temper | 222 W/(m·K)TYPICAL · O Temper | 34 MPaTYPICAL · O Temper · Drawn Tube | 90 MPaTYPICAL · O Temper · Drawn Tube | VERIFIED | |
| 2011 AluminumAA 2011 | Wrought Aluminum Alloys | 39 % IACSTYPICAL · T3 Temper | 151 W/(m·K)TYPICAL · T3 Temper | 296 MPaTYPICAL · T3 Temper · Cold Finished Rod & Bar | 379 MPaTYPICAL · T3 Temper · Cold Finished Rod & Bar | VERIFIED | |
| 2014 AluminumAA 2014 | Wrought Aluminum Alloys | 50 % IACSTYPICAL · O Temper | 192 W/(m·K)TYPICAL · O Temper | 97 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | 186 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | VERIFIED | |
| 2017 AluminumAA 2017 | Wrought Aluminum Alloys | 50 % IACSTYPICAL · O Temper | 193 W/(m·K)TYPICAL · O Temper | 70 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | 179 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | VERIFIED | |
| 2024 AluminumAA 2024 | Wrought Aluminum Alloys | 50 % IACSTYPICAL · O Temper | 190 W/(m·K)TYPICAL · O Temper | 76 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | 186 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | VERIFIED | |
| 3003 AluminumAA 3003 | Wrought Aluminum Alloys | 50 % IACSTYPICAL · O Temper | 193 W/(m·K)TYPICAL · O Temper | 41 MPaTYPICAL · O Temper · Drawn Tube | 110 MPaTYPICAL · O Temper · Drawn Tube | VERIFIED | |
| 5052 AluminumAA 5052 | Wrought Aluminum Alloys | 35 % IACSTYPICAL | 138 W/(m·K)TYPICAL | 90 MPaTYPICAL · O Temper · Drawn Tube | 193 MPaTYPICAL · O Temper · Drawn Tube | VERIFIED | |
| 6061 AluminumAA 6061 | Wrought Aluminum Alloys | 47 % IACSTYPICAL · O Temper | 180 W/(m·K)TYPICAL · O Temper | 55 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | 124 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | VERIFIED | |
| 6063 AluminumAA 6063 | Wrought Aluminum Alloys | 58 % IACSTYPICAL · O Temper | 218 W/(m·K)TYPICAL · O Temper | 48 MPaTYPICAL · O Temper · Drawn Tube | 90 MPaTYPICAL · O Temper · Drawn Tube | VERIFIED | |
| 7050 AluminumAA 7050 | Wrought Aluminum Alloys | 39.5 % IACSTYPICAL · T76, T76511 Temper | 154 W/(m·K)TYPICAL · T76, T76511 Temper | 469 MPaTYPICAL · T7451 Temper · Plate · LONGITUDINAL | 524 MPaTYPICAL · T7451 Temper · Plate · LONGITUDINAL | VERIFIED | |
| 7075 AluminumAA 7075 | Wrought Aluminum Alloys | 45 % IACSTYPICAL · O Temper | 173 W/(m·K)TYPICAL · O Temper | 103 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | 228 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | VERIFIED | |
| 7175 AluminumAA 7175 | Wrought Aluminum Alloys | 33 % IACSTYPICAL · T66 Temper | 130 W/(m·K)TYPICAL · T66 Temper | 510 MPaTYPICAL · T66 Temper · Forgings | 572 MPaTYPICAL · T66 Temper · Forgings | VERIFIED | |
| 7475 AluminumAA 7475 | Wrought Aluminum Alloys | 36 % IACSTYPICAL · T651 Temper | 142 W/(m·K)TYPICAL · T651 Temper | 510 MPaTYPICAL · T651 Temper · Sheet & Plate | 586 MPaTYPICAL · T651 Temper · Sheet & Plate | VERIFIED |