Verified Production Database
Materials Catalog & Specifications
Explore verified copper, steel, and stainless steel materials. Coverage varies by grade; inspect source-specific chemistry, conditions, and limits before selecting a material.
Filter Material Subfamily:Clear Filters
All Materials (105)Austenitic (14)Ferritic (1)Martensitic (2)Precipitation Hardening (1)Carbon Steel (14)Alloy Steel (16)Tool Steel (0)Wrought Aluminum Alloys (27)Cast Aluminum Alloys (0)Pure Copper (3)Deoxidized Copper (3)Free-Machining Copper (2)Beryllium Copper (3)High-Performance Copper Alloys (1)Cartridge Brass (1)Yellow Brass (4)Free-Machining Brass (1)Naval Brass (1)Phosphor Bronze (3)Aluminum Bronze (4)Silicon Bronze (1)Copper-Nickel (Cupronickel) (2)Bearing Bronze (1)Brass (General) (0)Bronze (General) (0)Alpha-Beta Titanium Alloys (0)Commercially Pure Titanium (0)Gray Cast Iron (0)Ductile (Nodular) Iron (0)Corrosion-Resistant Alloys (0)Nickel-Based Superalloys (0)
14 Material Records Qualified
| Designation • Canonical Grade | Subfamily | Standard Identifiers | Conductivity (% IACS) | Yield & Context | Density | Status | Actions |
|---|---|---|---|---|---|---|---|
| 201 Stainless Steel | Austenitic | TYPE: 201SPECIFICATION: 201 Stainless Steel Engineering Datasheet | — | ≥ 310 MPaMINIMUM · Annealed · Sheet and Strip | 7.81 g/cm³TYPICAL | VERIFIED | |
| 202 Stainless Steel | Austenitic | TYPE: 202SPECIFICATION: 202 Stainless Steel Engineering Datasheet | — | ≥ 310 MPaMINIMUM · Annealed · Sheet and Strip | 7.8 g/cm³TYPICAL | VERIFIED | |
| 301 Stainless Steel | Austenitic | TYPE: 301SPECIFICATION: 301 Stainless Steel Engineering Datasheet | — | ≥ 276 MPaMINIMUM · Annealed · Sheet and Strip | 7.88 g/cm³TYPICAL | VERIFIED | |
| 302 Stainless Steel | Austenitic | TYPE: 302SPECIFICATION: 302 Stainless Steel Engineering Datasheet | — | ≥ 205 MPaMINIMUM · Annealed · Sheet and Strip | 7.9 g/cm³TYPICAL | VERIFIED | |
| 303 Stainless Steel | Austenitic | TYPE: 303SPECIFICATION: 303 Stainless Steel Engineering Datasheet | — | ≥ 205 MPaMINIMUM · Cold Finished Annealed Bar · Bar | 7.9 g/cm³TYPICAL | VERIFIED | |
| 304 Stainless Steel | Austenitic | TYPE: 304UNS: S30400SPECIFICATION: 304 Stainless Steel Engineering Datasheet | — | ≥ 206.8 MPaMINIMUM · ASTM requirements (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. | 7.9 g/cm³TYPICAL · Published metric value; no test temperature stated. | VERIFIED | |
| 304L Stainless Steel | Austenitic | TYPE: 304LUNS: S30403SPECIFICATION: 304L Stainless Steel Engineering Datasheet | — | ≥ 172.4 MPaMINIMUM · ASTM requirements (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. | 7.9 g/cm³TYPICAL · Published metric value; no test temperature stated. | VERIFIED | |
| 305 Stainless Steel | Austenitic | TYPE: 305SPECIFICATION: 305 Stainless Steel Engineering Datasheet | — | ≥ 170 MPaMINIMUM · Annealed · Sheet and Strip | 7.9 g/cm³TYPICAL | VERIFIED | |
| 309 Stainless Steel | Austenitic | TYPE: 309SPECIFICATION: 309 Stainless Steel Engineering Datasheet | — | ≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip | 7.9 g/cm³TYPICAL | VERIFIED | |
| 310 Stainless Steel | Austenitic | TYPE: 310SPECIFICATION: 310 Stainless Steel Engineering Datasheet | — | ≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip | 7.9 g/cm³TYPICAL | VERIFIED | |
| 316 Stainless Steel | Austenitic | TYPE: 316UNS: S31600SPECIFICATION: 316 Stainless Steel Engineering Datasheet | — | ≥ 206.8 MPaMINIMUM · ASTM requirements at room temperature (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. Source specifies room temperature without a numeric temperature. | 7.9 g/cm³TYPICAL · Published metric value; no test temperature stated. | VERIFIED | |
| 316L Stainless Steel | Austenitic | TYPE: 316LUNS: S31603SPECIFICATION: 316L Stainless Steel Engineering Datasheet | — | ≥ 172.4 MPaMINIMUM · ASTM requirements at room temperature (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. Source specifies room temperature without a numeric temperature. | 7.9 g/cm³TYPICAL · Published metric value; no test temperature stated. | VERIFIED | |
| 321 Stainless Steel | Austenitic | TYPE: 321SPECIFICATION: 321 Stainless Steel Engineering Datasheet | — | ≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip | 7.9 g/cm³TYPICAL | VERIFIED | |
| 347 Stainless Steel | Austenitic | TYPE: 347SPECIFICATION: 347 Stainless Steel Engineering Datasheet | — | ≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip | 7.96 g/cm³TYPICAL | VERIFIED |