Intent: Continuous 200°C thermal endurance, aggressive synthetic fuels, and aromatic solvent resistance of FKM versus wide thermal span (-60°C to +200°C), biological inertness, and food/medical compliance of VMQ.
Engineering Verdict & When to Choose Each
FKM or silicone: separate fluid compatibility from thermal flexibility
By Mat Grades Editorial Desk · Updated 2026-11-14
FKM and VMQ silicone can be shortlisted for different sealing problems, but neither family name defines a complete compound. Begin with fluid chemistry, pressure, movement and the full temperature cycle. Do not choose the more expensive family simply because it is associated with demanding service.
A dry-air temperature statement is not proof of compatibility in hot liquid, fuel or steam. Likewise, a flexible sample is not evidence that a gland will seal at cold start. Obtain compound-specific data and a representative assembly test where leakage matters.
The catalog currently has no verified numeric property rows for FKM. That gap must remain visible rather than being filled from a generic temperature range or another compound. For VMQ, read each available value in its own context. Compare formulation, hardness, dimensional tolerances and any required product approvals on the supplier documentation before release.
Fluoroelastomer (FKM): evidence to check
Fluoroelastomer (FKM) has 0 cataloged property rows. No verified numeric rows are available, so compound-specific supplier data is needed before a numerical comparison. The record identifies ASTM D1418; check its scope and ordered edition. These are source-scoped examples rather than unrestricted design allowables. Read the full row context and certificate before using a value for acceptance; an absent value is not zero or a performance failure.
Silicone Rubber (VMQ): evidence to check
Silicone Rubber (VMQ) has 1 cataloged property rows. Compression Set (22h at 150°C) is reported as 10–25 % (range; Platinum-Cured Liquid Silicone Rubber (Post-Cured 4h at 200°C), tested at 150 °C). The record identifies ASTM D1418; check its scope and ordered edition. These are source-scoped examples rather than unrestricted design allowables. Read the full row context and certificate before using a value for acceptance; an absent value is not zero or a performance failure.
Four questions before approval
- Is the actual fluid mixture and exposure duration known?
- Do temperature claims apply to the same medium and duty?
- Is compound-specific evidence available for both candidates?
- Are required approvals attached to the supplied formulation?
Check the linked material records for the complete source trail. Read the methodology before comparing minimum requirements with typical measurements. No direct substitution or qualified fabrication procedure is implied.
Material Comparison
Compare verified engineering materials side by side with condition-specific mechanical properties.
| Parameter | Fluoroelastomer (FKM) | Silicone Rubber (VMQ) |
|---|---|---|
| Material Family | Rubber & Elastomers | Rubber & Elastomers |
| Subfamily | High-Temperature & Specialty Elastomers | High-Temperature & Specialty Elastomers |
| ASTM Designation | FKM | VMQ |
| ISO Designation | FPM | VMQ |
| ASTM-D2000 Designation | Type HK | Type FC / FE / GE |
| Element | Fluoroelastomer (FKM) | Silicone Rubber (VMQ) |
|---|
| Mechanical Parameter | Fluoroelastomer (FKM)Standard Bisphenol-Cured Compound (Post-Cured 16h at 230°C) | Silicone Rubber (VMQ)Platinum-Cured Liquid Silicone Rubber (Post-Cured 4h at 200°C) |
|---|---|---|
| Compression Set (22h at 150°C) · Platinum-Cured Liquid Silicone Rubber (Post-Cured 4h at 200°C) · RANGE · 150 °CUnit: % | — % | 10–25 % |
Machinability: Cryogenically deflashed with liquid nitrogen; turned on CNC lathes equipped with diamond-sharp carbide cutters.
Formability / Cold Working: Milled on cool water-chilled roll mills; compounded with mineral fillers and basic metal oxides (Ca(OH)₂ and MgO) as acid acceptors. Compression, transfer, and injection molded; extruded into chemical tubing.
Heat Treatment & Annealing: Bisphenol cure (standard Type 1) or peroxide cure (for aggressive sour gas/acid resistance). Mandatory oven post-cure at 230°C for 16 to 24 hours to complete crosslinking and achieve minimum compression set.
Machinability: Waterjet cutting and precision rotary die cutting; cryogenic machining used for custom surgical prototypes.
Formability / Cold Working: High-consistency rubber (HCR) is milled and molded via compression, transfer, and extrusion; liquid silicone rubber (LSR) is processed via two-component high-speed meter-mix liquid injection molding.
Heat Treatment & Annealing: Vulcanized via organic peroxide catalysts (for HCR) or platinum-catalyzed hydrosilylation addition cure (for LSR). Post-curing at 200°C for 2 to 4 hours is mandatory to volatilize cyclic siloxanes and optimize compression set.